1.1 These test methods cover the chemical analysis of ferroniobium having chemical compositions within the following limits:

Element Concentration, %
Aluminum 2.00 max
Carbon 0.30 max
Chromium 2.00 max
Cobalt 0.25 max
Lead 0.01 max
Manganese 3.00 max
Niobium 40.00 to 75.00
Phosphorus 0.05 max
Silicon 4.00 max
Sulfur 0.03 max
Tantalum 7.00 max
Tin 0.15 max
Titanium 5.00 max
Tungsten 0.50 max

1.2 The test methods appear in the following order:

Sections
Separation of Niobium, Tantalum, and Titanium
by the Ion-Exchange Test Method
10-16
Titanium by the Photometric Test Method [0.05 % to 5.0 %] 17-21
Niobium by the Gravimetric Test Method [40 % to 75 %] 22-23
Tantalum by the Gravimetric Test Method [1 % to 7 %] 24-25
Tantalum by the Photometric Test Method [0.25 % to 1 %] 26-30

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 6, and specific warning statements in 11.1.

10.1 These test methods cover the determination of niobium, tantalum, and titanium in ferroniobium from 40 % to 75 %, 0.25 % to 7 %, and 0.05 % to 5.0 %, respectively.